E-Polymers TEKAMID® TA250FR , Flame Retardant Un-Reinforced PA66, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® TA250FR , Flame Retardant Un-Reinforced PA66, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardantInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D786
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 260 °C
500 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 265 - 285 °C
509 - 545 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F