Material Notes:
GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D786
Tensile Strength, Yield 125 MPa
18100 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 190 MPa
27600 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F