Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAPPO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance and reinforced fiberglass. It shows high dimensional stability and rigidity used for housing and electrical parts.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength 71.613 MPa
10387 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 112.82 MPa
16363 psi
ASTM D790
Flexural Modulus 2.6487 GPa
384.16 ksi
ASTM D790
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 280 - 310 °C
536 - 590 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Users viewing this material also viewed the following: