Material Notes:
ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. This mold material has proven to be highly effective for injection molding, blow molding, thermoforming, and other plastic processing applications.ECOMold® 95 is used in applications requiring a high thermal conductivity level such as cores, core inserts, cavities - inserts, core pins, blow pins, ejector pins, lifters, sleeves, and sprue bushings.Information provided by ECOMold.
Physical Properties Metric English Comments
Density 8.72 g/cc
0.315 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 210
210
3000 kg
Hardness, Rockwell B 94
94
Tensile Strength, Ultimate 689 MPa
100000 psi
Tensile Strength, Yield 372 MPa
54000 psi
Proportional Limit
517 MPa

@Strain 0.200 %
75000 psi

@Strain 0.200 %
Elongation at Break 13 %
13 %
in 2"
Modulus of Elasticity 110 GPa
16000 ksi
Tension
Compressive Strength 552 MPa
80000 psi
0.1% Permanent Set
Charpy Impact 33.9 J
25.0 ft-lb
V-Notch
Thermal Properties Metric English Comments
CTE, linear 17.5 µm/m-°C

@Temperature 20.0 °C
9.70 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 233 W/m-K
1620 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000380 ohm-cm
<= 0.00000380 ohm-cm