Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Pacific Sintered Materials FX-233-T Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Kennametal Stellite Deloro® 208 PM after P/M Processing Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |
|||
Tensile Strength, Ultimate | 690 MPa @Temperature 649 °C |
100000 psi @Temperature 1200 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | statistical analysis gives AVG -3STD at 626 MPa |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
MetalTek MTEK 420 Cast UNS J91153 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
MetalTek MTEK SD100 Cast UNS J93380 Duplex Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
MetalTek FERRALIUM® 225 UNS J32550 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels. Produced under license of Meighs Ltd.Applications: Offshore piping systems, couplings. Cen.. |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, v.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 2.0 inc.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | Heat Treated |
Universal Wire Works 29-9 (AMS 5784) Filler Metal Universal 29-9 is designed for welding similar and dissimilar corrosion and heat resisting steels with the gas metal arc and gas tungsten arc welding processes.Information provided by Universal Wire.. |
|||
Tensile Strength, Ultimate | 689 - 786 MPa | 100000 - 114000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | annealed |
CMW® ELKONIUM 32 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 405 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 41 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 42 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 690 - 800 MPa | 100000 - 116000 psi | |
ArcelorMittal TRIP 690 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT690T), electrogalvanized (HCT690T+ZE) and Extragal®/Galvannealed (HCT690T+Z)Description: TRIP steels offer an outstanding combination of strength and ductil.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allvac® Nickelvac® 600 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Aircraft engines, nuclear reactor applications, chemical process equipment, high temperature fixtures. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal Data provided by Allvac.Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Data provided by Allvac.Applications: Afterburner components, combustion chamber liners, nozzles, vanes, rings, turbine exhaust weldments, structural parts. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allvac® Vasco® 410/403 Specialty Steel, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Compressor blades, turbine parts. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allvac® 3-2.5 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | typical |
ATI Allegheny Ludlum AL 825™ Nickel Alloy Allegheny Ludlum AL 825 alloy is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of corrosion resistance to both moderately oxidizing and moderately reducing enviro.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |