Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 517 MPa @Temperature 23.9 °C |
75000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Aramid Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
Performance Alloys MoldStar® 150 (PAS 940) Copper Mold Alloy Description: MoldStar® 150 is a high-performance, beryllium-free copper alloy for the blow molding and injection molding industries. In addition to its high thermal conductivity, MoldStar® 150 off.. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 %, Temperature 538 °C |
75000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate 13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 1400°F for 2 hrs and 1150°F for 4 hrs |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Tensile Strength, Yield | 517 MPa @Temperature 24.0 °C |
75000 psi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric Hexcel designation: K285-38"-F522; Kev. 49 1140Information provided by HexCel |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 301 Austenitic Stainless Steel, 1/4 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 302 Austenitic Stainless Steel, 1/4 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 305 Austenitic Stainless Steel, 1/4 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, 1/4 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% offset |
Eagle Brass 7026 Copper Nickel, 1/4 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% offset |
Eagle Brass 70265 XP175, 1/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 517 - 621 MPa | 75000 - 90000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 517 MPa | >= 75000 psi | 0.2% Offset |
Eagle Brass 304L Austenitic Stainless Steel, 1/4 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® 35N Nickel Superalloy, Heat Treatment: 1052°C (1925°F) + Age Data provided by Allvac.Applications: Aircraft fasteners. Line wire for down-hole instrumentation. Biomedical devices, high fatigue strength applications. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® C-263 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Ring components in jet engines. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal Data provided by Allvac.Applications: Aerospace rings, forgings, weld wire. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® N-90 Nickel Superalloy, Heat Treatment: 1066°C (1950°F) + Age Data provided by Allvac.Applications: Turbine blades and other jet engine components. Valves for internal combustion engines. |
|||
Tensile Strength, Yield | >= 517 MPa @Strain 0.200 % |
>= 75000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Tensile Strength, Yield | 517 MPa | 75000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 10% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Yield | 517 MPa @Strain 0.200 % |
75000 psi @Strain 0.200 % |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |