Material Notes:
Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important properties: Excellent adhesion to thermoplastic elastomersHigh stiffnessGood impact strength Application examples: Automotive plugs and seals, counter wheel sensors, housings with integrated switch membranes, housings (hard soft combinations), grip handles, and plug housings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Water Absorption 2.5 %
2.5 %
ISO 62
Moisture Absorption 1.00 %
1.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
conditioned; ISO 527-1/-2
85.0 MPa
12300 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
3.0 %
3.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 4.90 GPa
711 ksi
conditioned; ISO 527-1/-2
6.40 GPa
928 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
dry; ISO 179/1eU
3.50 J/cm²
16.7 ft-lb/in²
conditioned; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
3.50 J/cm²

@Temperature 30.0 °C
16.7 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
0.900 J/cm²
4.28 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 26.0 kV/mm
660 kV/in
conditioned; IEC 60243-1
27.0 kV/mm
686 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Form Granules
Industry & Consumer goods Heating systems
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics High impact or impact modified