EMS-Grivory Grivory® LV-23 X ESD PA12-GF23

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 20% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® LV-23 X ESD PA12-GF23.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 Ohmgood fuel and zinc chloride resistancegood surface qualityheat resistanthigh impactgood processability Applications requiring antistatic properties such as fuel system quick connectors, valve housings, structural parts of safety devices and instruments requiring ESD protection.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Water Absorption 1.2 %
1.2 %
ISO 62
Moisture Absorption 0.500 %
0.500 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 115 MPa
16700 psi
conditioned; ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
conditioned; ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 5.50 GPa
798 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
conditioned; ISO 179/1eU
3.50 J/cm²

@Temperature 30.0 °C
16.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
conditioned; ISO 179/1eA
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
conditioned; IEC 60093
Surface Resistance 1000 ohm
1000 ohm
IEC 60093
Descriptive Properties Value Comments
Automotive Fuel systems
Form Granules
Processing Injection Molding
Product Attributes Hydrolysis resistant
Special Characteristics Anti-static
High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following: