Polymer Property : Deflection Temperature at 8.0 MPa = 230 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
ISO 75-C
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
ISO 75-C
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
ISO 75-C
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 175
Perstorp Compounds Aminel FX Melamine
Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp ..
Deflection Temperature at 8.0 MPa >= 110 °C
>= 230 °F
ISO 175
Perstorp Compounds AMITEC 751 Melamine
Perstorp dinnerware compression and injection grade. Porcelain like properties suitable for household applications.Information provided by Perstorp Compounds Inc.
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-2
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive  (discontinued **)
Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-2
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage  (discontinued **)&
Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-2
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber
30% Glass fiber reinforced; injection molding grade
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1,-2
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS.
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30
Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23
Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30
Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 4106 nat PA612-GF30
Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 110 - 130 °C
230 - 266 °F
Injection and Compression; ISO 75-C
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
Deflection Temperature at 8.0 MPa 110 - 140 °C
230 - 284 °F
Average value: 123 °C Grade Count:11
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-2
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures  (discontinued **)
Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50
Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine..
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50
Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..