EMS-Grivory Grivory® XE 4158 nat PA612

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4158 nat PA612.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGood heat stabilityHigh UV- and weathering resistanceSuper high cold impact strengthGood chemical resistanceGood surface finishGood dimensional stabilityLow density Grilamid XE 4158 natural is suitable for the extrusion of profiles and tubes for applications in automotive and industrial markets. In addition it can be used for injection molding applications such as winter sport items for which high impact strength at low temperatures is required.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Water Absorption 1.3 %
1.3 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
dry, 15s; ISO 868
65
65
conditioned, 15s; ISO 868
Tensile Strength, Yield 30.0 MPa
4350 psi
dry; ISO 527-1/-2
30.0 MPa
4350 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 13 %
13 %
dry; ISO 527-1/-2
18 %
18 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
1.00 GPa
145 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 8.50 J/cm²
40.4 ft-lb/in²
dry; ISO 179/1eA
8.50 J/cm²
40.4 ft-lb/in²
conditioned; ISO 179/1eA
4.00 J/cm²

@Temperature 30.0 °C
19.0 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 210 µm/m-°C
117 µin/in-°F
ISO 11359-1/-2
Melting Point 179 °C
354 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 100 °C
194 - 212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 40.0 kV/mm
1020 kV/in
dry; IEC 60243-1
40.0 kV/mm
1020 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Compressed air systems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Other Extrusion
Product Attributes Flexible
Hydrolysis resistant
Improved alcohol resistance
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)