Eagle Brass 102 OF COPPER (Non-Certified), Annealed

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 102 OF COPPER (Non-Certified), Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance and is used for high current applications.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Annealed
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 179 - 262 MPa
26000 - 38000 psi
Tensile Strength, Yield 41.4 - 89.6 MPa
6000 - 13000 psi
0.2% offset
Elongation at Break 20 - 50 %
20 - 50 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.6 µm/m-°C

@Temperature 20.0 - 300 °C
9.80 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu >= 99.9 %
>= 99.9 %
Oxygen, O <= 0.0010 %
<= 0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed