Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Nylene® 9643 , 43% Glass Reinforced Nylon 6,6/6 Description: Nylene® 9643 is a 43 % glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Reso.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
  AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® RA-20CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-20CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SF-30CF/000 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 179 MPa @Temperature 982 °C |
26000 psi @Temperature 1800 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 179 - 262 MPa | 26000 - 38000 psi | |
Eagle Brass 110 EPT COPPER, Annealed Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | |
Dow Saran® 510 PVDC SARAN® 510 resin is a copolymer of vinylidene chloride and vinyl chloride, supplied as a white free flowing powder (particle size 250 microns). It is a formulated polymer designed for extrusion int.. |
|||
Tensile Strength, Ultimate | 179 - 262 MPa | 26000 - 38000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Annealed Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 179 - 262 MPa | 26000 - 38000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Annealed Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | annealed |
CMW® ELKONIUM 46 Silver Alloy The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low cont.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Adell BR-38 Nylon 6, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ASTM D638 |
Adell BR-18 Nylon 6, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ATSM D638 |
Ashley Polymers Ashlene® 520-40G Nylon 66, 40% Glass Reinforced A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ATSM D638 |
Ashley Polymers Ashlene® 830LS-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced and heat stabilized Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 t.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | 10 oz glass cloth laminate |
BCC Products BC 5114 Epoxy Laminating System BC 5114 is a gray low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use abov.. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 179 MPa | 26000 psi | ATSM D638 |
Ashley Polymers Ashlene® 830L-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |