Material Notes:
Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.89 g/cc
0.285 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 1030 MPa
>= 150000 psi
Tensile Strength, Yield >= 758 MPa
>= 110000 psi
0.2% Offset
Elongation at Break >= 9.0 %
>= 9.0 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.7 µm/m-°C

@Temperature 20.0 - 649 °C
10.4 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 16.3 W/m-K
113 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 17 - 19 %
17 - 19 %
Iron, Fe 68.025 - 75 %
68.025 - 75 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 8.0 - 10 %
8.0 - 10 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %