Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.89 g/cc
0.285 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 862 MPa
>= 125000 psi
Tensile Strength, Yield >= 517 MPa
>= 75000 psi
0.2% Offset
Elongation at Break >= 10 %
>= 10 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.7 µm/m-°C

@Temperature 20.0 - 649 °C
10.4 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 16.3 W/m-K
113 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 18 - 20 %
18 - 20 %
Iron, Fe 66.595 - 74 %
66.595 - 74 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 8.0 - 10.5 %
8.0 - 10.5 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %