Material Notes:
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 except that this alloy is somewhat stronger at elevated temperatures. Corrosion resistance is improved, particularly against sulfuric, hydrochloric, acetic, formic, and tartaric acids; acid sulfates and alkaline chlorides.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 689 MPa
>= 100000 psi
Tensile Strength, Yield >= 379 MPa
>= 55000 psi
0.2% Offset
Elongation at Break >= 30 %
>= 30 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.5 µm/m-°C

@Temperature 20.0 - 649 °C
10.3 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 15.9 W/m-K
110 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 16 - 18 %
16 - 18 %
Iron, Fe 62.095 - 72 %
62.095 - 72 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
2.0 - 3.0 %
Nickel, Ni 10 - 14 %
10 - 14 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %