Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 241 °C | 466 °F | |
Plastcom SLOVAMID 6 NG GF 20 HLS PA6, 20% glass fibre, combined stability FeaturesPA 6 for injection moulding, chemically reinforced with 20% glass fibre, heat stabilized and weather stabilized. Stabilized against hydrolysis. Good surface finisch.Packaging, transport, sto.. |
|||
Melting Point | 241 °C | 466 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman BD445 PET
(discontinued **) Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This pol.. |
|||
Melting Point | 241 °C | 466 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |
|||
Melting Point | 241 °C | 466 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Melting Point | 241 °C | 466 °F | |
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 241 °C | 466 °F | DIN 53736; ASTM D789 |
Kolon NOPLA® KE531 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Melting Point | 241 - 248 °C | 466 - 478 °F | |
Indium Corp. Indalloy® 264 Tin-Antimony Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Melting Point | 241 °C | 465 °F | ASTM D-3418 |
Saint-Gobain Norton® ECTFE Fluoropolymer Film Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon.. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Melting Point | 241 °C | 466 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® B90A PET Laser+® (B90A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Bi-orientation of Laser+® (B.. |
|||
Melting Point | 241 °C | 466 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® B90B PET Product Description: Laser+® (B90B) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typical .. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Melting Point | <= 241 °C | <= 466 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Melting Point | 241 °C | 466 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® W P41A PET Product Description: Laser+® W (P41A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Melting Point | 241 °C | 465 °F | ASTM D4591 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |