Eastman D4042-P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman D4042-P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
D4042-P is a low density resin designed for applications such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seals at high packaging or sealing ratesList of Applications:Food packagingFreezer wrapFrozen food packagingSugar pouchesInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D4883
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Tensile Strength, Yield 9.00 MPa
1310 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Elongation at Break 300 %
300 %
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating