Ensinger TECAFINE™ PP Polypropylene (PP)

Category Polymer , Thermoplastic , Polyolefin , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ensinger
Trade Name TECAFINE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECAFINE™ PP Polypropylene (PP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAFINE™ PP is an anti-stated, polypropylene, random copolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical properties than other typical polyolefin materials, it is light weight, weldable, and unaffected by moisture. Ensinger's processing technology provides quality in TECAFINE™ PP stock shapes.Excellent chemical resistance (TECAFINE™ PP is resistant to organic chemicals, solvents, mineral acids, and inorganic salts)WeldableHigh purity (nonparticulating and suitable for high purity environments)FDA compliant (meets FDA 21 DFR 177.1520)Light wieght (has a specific gravity of less than 1)Moisture resistant (unaffected by water or moist environments)Great quality (Ensinger's extrusion expertise means users consistently obtain the highest quality polypropylene stock shapes)TECAFINE™ PP's excellent chemical resistance and high purity characteristics make it ideal for use in the food-processing and chemical-procesing industries. Common applications include pump and valve components, tanks, laboratory equipment, and other parts in contact with corrosive environments.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Density 0.913 g/cc
0.0330 lb/in³
ASTM D792
Water Absorption 0.010 - 0.030 %

@Temperature 22.8 °C,
Time 86400 sec
0.010 - 0.030 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength at Break 32.4 MPa

@Temperature 22.8 °C
4700 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 100 %

@Temperature 22.8 °C
100 %

@Temperature 73.0 °F
ASTM D638
Tensile Modulus 0.896 GPa

@Temperature 22.8 °C
130 ksi

@Temperature 73.0 °F
ASTM D638
Flexural Strength 41.4 - 55.2 MPa

@Temperature 22.8 °C
6000 - 8000 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 1.24 GPa

@Temperature 22.8 °C
180 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 22.8 °C
0.900 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Melting Point 166 °C
330 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm

@Temperature 22.8 °C
1.00e+17 ohm-cm

@Temperature 73.0 °F
ASTM D257
Dielectric Constant 2.2

@Frequency 60.0 Hz,
Temperature 22.8 °C
2.2

@Frequency 60.0 Hz,
Temperature 73.0 °F
50% RH; ASTM D150