Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECAPRO™ SAN Polypropylene (PP)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ensinger
Trade Name TECAPRO™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECAPRO™ SAN Polypropylene (PP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial additive. These silver ions are released gradually to reduce the formation of bacterial.Less bacterial contaminationReduced odor and biofilm formationDiminished formation of bacteria in equipmentActive components are harmless to humansScrubbing surface renews antimicrobial effectFDA conformity of raw material, color pigments and antimicrobial additiveTECAFORM™ SAN and TECAPRO™ SAN are ideal where continual sanitary and anti bacterial conditions are a requirement. Excellent for components in food processing equipments, bottling and canning machines, water handling and filtration equipment. Door handels and buttons in public places would benefit from reduction in transfer of bacteria. TECAPRO™ SAN is especially effective in surgical instruments, trays, work surfaces and cutting boards in medical as well as food storage and preparation areas.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.050 %

@Temperature 22.8 °C
0.050 %

@Temperature 73.0 °F
equilibrium, 50% RH; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 100 MPa
14500 psi
ISO 2039/1,2
Tensile Strength, Yield 32.99 MPa
4785 psi
ASTM D638, DIN EN ISO 527
Elongation at Break >= 30 %
>= 30 %
ASTM D638, ISO 527
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790, ISO 178
Izod Impact Resistance 0.0689 J/cm²
0.328 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
DIN 53 736
Maximum Service Temperature, Air 100 °C
212 °F
Long Term
121 °C
250 °F
Sort Term
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
ISO - 75/A
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: