Polymer Property : Compressive Strength = 31200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 215 MPa
31200 psi
ASTM D695
Premix Premi-Glas® 1200-30 Polyester SMC
Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac..
Compressive Strength 215 MPa
31200 psi
ASTM D695
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
Compressive Strength 215 MPa
31200 psi
ASTM D695
Glastic Laminates/Shapes 1580 Polyester Laminate
Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements.
Compressive Strength 215 MPa
31200 psi
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK
LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding.
Compressive Strength 215 MPa
31200 psi
ASTM D695
Plenco 2567 Phenolic, Granular, Compression Molded
PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo..
Compressive Strength 215 MPa
31200 psi
ASTM D695
Plenco 5482 Phenolic, Granular, Transfer Molded
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect..
Compressive Strength 215 MPa
31200 psi
ASTM D695
Plenco 6015 Phenolic, Briquette, Transfer Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
Compressive Strength 215 MPa
31200 psi
ASTM D695
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle..
Compressive Strength 215 MPa
31200 psi
Abatron AboCast 8504-1 One-Component Epoxy
AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications.
Compressive Strength 215 MPa
31200 psi
ISO 604
Sumitomo Bakelite North America RX® 852 Novolac Phenolic
Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group