Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-98 Medical Compression Molded PEEK Compound, 30% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-98 Medical Compression Molded PEEK Compound, 30% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ASTM D785
Hardness, Shore D 93
93
ASTM D2240
Tensile Strength 126 MPa
18300 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
Flexural Strain; ASTM D790
2.2 %
2.2 %
ASTM D638
Tensile Modulus 9.65 GPa
1400 ksi
ASTM D638
Flexural Strength 210 MPa
30500 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength <= 179 MPa
<= 26000 psi
ASTM D695
Compressive Modulus 4.14 GPa
600 ksi
ASTM D695
Shear Strength 83.4 MPa
12100 psi
ASTM D732
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 28.4 µm/m-°C
15.8 µin/in-°F
ASTM E831
Melting Point 343 °C
649 °F
DSC
Heat Distortion Temperature >= 237 °C
>= 459 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black