Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Epoxy Novolac 27%, Carbon fabric 73%

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxy Novolac 27%, Carbon fabric 73%.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Epoxy Novolac - Dow Chemical "DEN 438". Carbon fabric - "VCA"
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 64.19 MPa
9310 psi
Flexural Yield Strength 110 MPa
16000 psi
Flexural Modulus 6.41 GPa
930 ksi
Compressive Yield Strength 115 MPa
16700 psi
Compressive Modulus 8.20 GPa
1190 ksi
Users viewing this material also viewed the following: