Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Staramide RF007ESS PA66/6, 35% Glass Filled, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 40% Glass Fiber Reinforced
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide RF007ESS PA66/6, 35% Glass Filled, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Staramide RF007ESS is a 35% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as RF1007EMHS)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 178 MPa
25800 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
5 mm/min; ISO 527
Flexural Strength 235 MPa
34100 psi
2 mm/min; ISO 178
Flexural Modulus 9.10 GPa
1320 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80x10x4; ISO 179/1eA
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 237 °C
459 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 260 - 280 °C
500 - 536 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 290 °C
518 - 554 °F
Melt Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Moisture Content 0.20 %
0.20 %