ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name Enable™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Enable 20-10 resins are available with blown film formulations, with or without antiblock. A heavily stabilized formulation for cast film processing is also available. Availability: Africa & Middle East, Asia and EuropeAdditive:Antiblock: NoSlip: NoProcessing Aid: NoThermal Stabilizer: YesApplications: Agricultural FilmBlown FilmCast FilmCast Stretch FilmCollation ShrinkFood packagingForm Fill and Seal PackagingHeavy Duty BagsLamination FilmMultilayer Packaging FilmShrink FilmStand Up PouchesStretch Film Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa
1500 psi
ASTM D882
Film Elongation at Break, MD 540 %
540 %
ASTM D882
Film Elongation at Break, TD 740 %
740 %
ASTM D882
Puncture Energy 3.39 J
2.50 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 110 g
110 g
ASTM D1922
Elmendorf Tear Strength TD 570 g
570 g
ASTM D1922
Dart Drop Test 200 g
0.441 lb
ASTM D1709
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
ASTM D882
Film Tensile Strength at Break, TD 51.0 MPa
7400 psi
ASTM D882
1% Secant Modulus, MD 200 MPa
29000 psi
ASTM D882
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 239 °C
<= 462 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 7.6 %
7.6 %
ASTM D1003
Gloss 65 %
65 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 11 lbf
ExxonMobil Method