Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | ASTM D882 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
Westlake LF1020 Butene Linear Low Density Polyethylene Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05HH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Exceed™ 1023JA Metallocene Polyethylene Resin Product Description: Exceed 1023JA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1023JA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil LD 051.LQ Shrink Film Resin L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil NTX™ NTX 095 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil NTX™ NTX 104 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil NTX™ NTX 141 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil NTX™ NTX 150 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | |
Dow LDPE 683I Low Density Polyethylene, Film Grade DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1500 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 10.3 MPa | 1490 psi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Film Tensile Strength at Yield, TD | 10.3 - 13.0 MPa | 1500 - 1890 psi | Average value: 12.0 MPa Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |