Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
Melt Flow | 0.65 - 0.85 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 - 0.85 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) Arak 20075AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 0.65 g/10 min | 0.65 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 5625 LDPE Case Shrink and Bundling Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Superior Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, High Antiblock, Easy Openability, Medium Coefficient of Frictio.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Melt Flow | 0.65 g/10 min | 0.65 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg |
0.65 g/10 min @Load 4.76 lb |
ISO 1133 |
SIDPEC EGYPTENE® LL 2406 AA LLDPE Pipe Grade Applications:Drip irrigation pipeSmall potable water pipeInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake Tymax™ GT4524 Anhydride Modified Linear Low Density Polyethylene Westlake GT4524 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a c.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HB6007 Blow Molding HDPE HomopolymerApplications: Milk, distilled water, soft drink concentrate, fruit juice, etc.Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excell.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HP6000 Pipe HDPE High Density Polyethylene Homopolymer for Pipe Extrusion Formolene® HP6000 is a high quality product for homopolymer pipe extrusion applications. It has excellent stiffness and good stiffness prope.. |
|||
Melt Flow | 0.65 g/10 min | 0.65 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® EHM 6007 High Density Polyethylene High Density PolyethyleneCustomer Benefits: A blow molding grade rein that offers a high quality product for those critical food packaging jobs and good impact strength and stiffness.Applications: L.. |
|||
Melt Flow | 0.65 g/10 min | 0.65 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® K606 High Density Polyethylene High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ FL 00119 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00119 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Ap.. |
|||
Melt Flow | 0.65 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.65 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Melt Flow | 0.65 g/10 min | 0.65 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® K607 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to.. |