ExxonMobil Escorene® LD-728 High EVA Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-728 High EVA Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 2.0 g/10 min
2.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Hardness, Shore D 31
31
ASTM D2240
Tensile Strength, Ultimate 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 5.00 MPa
725 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0510 GPa
7.40 ksi
1% Secant, ASTM D790
Tensile Impact Strength 610 kJ/m²
290 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
Exxon Method
Vicat Softening Point 62.0 °C
144 °F
1000g; ASTM D-1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746