Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D412 |
Polymax® Maxelast® A9855B TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ISO 527 |
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: .. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D412 |
Precision Polymer Engineering E70Z Ethylene Propylene Rubber Peroxide cured, grey Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electri.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 150°C for 1,000 hrs; JIS-K-6251 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® A 3810 TPE Thermoplastic Elastomer Features:Heat Resistance, GoodThermal Stability, GoodForms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
Trelleborg B473 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
Trelleborg Commercial Neoprene® C722 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
Trelleborg R661 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 5.00 MPa @Temperature 21.1 °C |
725 psi @Temperature 70.0 °F |
Flatwise Tensile; After 500 hrs at 400°F (Weight loss = 0.75%); Composite Honeycomb Sandwich Performance; ASTM C 297 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 300 % |
725 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1960AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 300 % |
725 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1966AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 300 % |
725 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1970AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8785A S043 Polyurethane injection molding gradewith special UV stabilizersexcellent abrasion resistanceEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
|
Covestro Texin® 285 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
|
Covestro Texin® 990R Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
|
Daikin DAI-EL G-751 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent metal bonding and compression set.Infor.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FSS 601 R PVC, Soft Injection Molding Grade NAKAN FSS 601 R is a soft polyvinyl chloride compound developed for injection molding of transparent soling ( very clear ).ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
BASF Lucalen® A 3110 M Ethylene/Acrylate Copolymer Economical composite films together with PE-LD; primers for aluminum/steel composites; coatings for paper board, aluminum and steel (e.g. for pipes used to transport petroleum, gas, etc.)Data was co.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
BASF Lucalen® A 3110 M Q 270 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 50 mm/min |
Arkema Group Evatane® 1040 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and high mechanical properties. Examples: thin stretch film for food packaging, coex.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 50 mm/min |
Arkema Group Evatane® 1090 VN 3 Ethylene Vinyl Acetate Description: EVA copolymer made by high pressure tubular process.Applications:Grade for molding flexible articles.Examples: Closures, plugs, swimming flippers, toys.ISO data provided by the manufact.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
Trelleborg R660 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FEM 691 N PVC, Soft Extrusion Grade NAKAN FEM 691 N is a soft polyvinyl chloride compound developed for extrusion of tubes for haemodialysis, heparin and fistula needles, general purpose.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D638 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D638 |
ExxonMobil Escorene® LD-730 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |