ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty applications that require robust performance in conditions ranging from ambient to sub-zero temperatures.Availability: Latin America, North America and South America Additive: Antioxidant: YesApplications: Industrial ComponentsIndustrial PailsLawn & Garden AccessoriesQuality HousewaresStructural Foam ArticlesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ExxonMobil method
ESCR 10% Igepal® 4.0 hour
4.0 hour
F50; ASTM D1963B
Melt Flow 6.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D638
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
2% Secant; ASTM D790B
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790B
Izod Impact, Notched 0.491 J/cm

@Temperature -40.0 °C
0.920 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 270 °C
<= 518 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.1 °C
115 °F
ASTM D648B