ExxonMobil LD 206.48 Extrusion Coating Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LD 206.48 Extrusion Coating Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LD 206.48 is a extrusion coating grade, having good organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ExxonMobil Method
Melt Flow 8.5 g/10 min
8.5 g/10 min
ExxonMobil Method
Neck In 4.10 cm
1.61 in
at 100 m/min, 35 rpm, 295°C; ExxonMobil Method
4.40 cm
1.73 in
at 50 m/min, 35 rpm, 295°C; ExxonMobil Method
Drawdown 1.07 m/s
210 ft/min
at 65 rpm, 295°C; ExxonMobil Method
2.59 m/s
510 ft/min
at 35 rpm, 295°C; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 87.8 °C
190 °F
ASTM D1525