Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin America, North America and South America Additive: Antiblock: 1000 ppmSlip: 500 ppm Thermal Stabilizer: YesApplications: Coextrusion FilmsFoamsForm Fill and Seal PackagingFreezer FilmHigh Clarity FilmLamination FilmPoultry BagProduce BagsRice BagsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil method
Vinyl Acetate Content 5.5 %
5.5 %
ExxonMobil Method
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1000 ppm
1000 ppm
Slip Level 500 ppm
500 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 190 %
190 %
ASTM D882
Film Elongation at Break, TD 590 %
590 %
ASTM D882
Puncture Energy 1.36 J
1.00 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 160 g
160 g
ASTM D1922
Elmendorf Tear Strength TD 80 g
80 g
ASTM D1922
Dart Drop Test 170 g
0.375 lb
ASTM D1709A
Film Tensile Strength at Break, MD 248 MPa
36000 psi
ASTM D882
Film Tensile Strength at Break, TD 24.1 MPa
3500 psi
ASTM D882
1% Secant Modulus, MD 124 MPa
18000 psi
ASTM D882
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 216 °C
<= 421 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
ASTM D1003
Gloss 74 %
74 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 11 lbf
ExxonMobil Method
Users viewing this material also viewed the following: