Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Network Polymers NPP 11-3225 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips 5455 LDPE Clear, General Purpose Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Clarity, High Gloss, Good Openability, Good Sealability, Suited for High Speed ConvertingApplications:Bakery and Food Products, Rack and Counter Merchand.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ISO 1183 |
LyondellBasell Lupolex FA LLDPE Description: Lupolex 25G FA is a linear low density polyethylene (LLDPE) used for blending, film, packaging, and bagsFeatures: AntioxidantGood Puncture ResistanceHigh RigidityHigh ClarityGood Heat S.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Density | 0.925 - 0.950 g/cc | 0.0334 - 0.0343 lb/in³ | ASTM D1505 |
Micropol Microlink XL Crosslinkable Polyethylene Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Lushan EP253H Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D-1505 |
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 306.57 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1201KG Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 6100.17 Linear Low Density Polyethylene Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2083G Linear Low Density Polyethylene Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2083G Linear Low Density Polyethylene Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D-1505 |
Bapolene® 108A Low Density Polyethylene Film Extrusion Resin Bapolene® 108A is an LDPE for blown film. It contains 2500 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | |
Arkema Group Evatane® 1005 VN 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process.Applications Grade for transparent and resistant film production. Examples: curtain stretch, coextrusion, stretch hood.ISO data provided by the ma.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Bapolene® 2272 Polyethylene, Injection Grade Bapolene LL2272 is a high flow, narrow molecular weight distribution, linear low density polyethylene injection resin. This resin offers excellent stress cracking resistance, flex life, low tempera.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3201.22 Premium High Strength Film Resin
(discontinued **) LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Density | 0.925 - 0.927 g/cc | 0.0334 - 0.0335 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |