Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 253 °C | 487 °F | ASTM D789 |
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | 253 °C | 487 °F | ASTM D789 |
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | 253 - 257 °C | 487 - 495 °F | QCD--W1-49 |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Melting Point | 253 - 257 °C | 487 - 495 °F | QCD--W1-49 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE L L6101RQ Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1201KG Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1201XV Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6101RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6101XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6201RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6201XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6201XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Melting Point | <= 253 °C | <= 487 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 2227ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2227ED is a metallocene ethylene-hexene copolymer. It offers an excellent balance of high modulus and impact strength. The higher melt index makes it ideally suited for L.. |