Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have good gloss and offer advantages in toughness, environmental stress crack resistance, stiffness and heat distortion resistance over comparable low density polyethylene items. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: Yes Applications: CompoundingHousewaresLidsThin Wall ArticlesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ExxonMobil method
ESCR 10% Igepal® 6.0 hour
6.0 hour
ASTM D1693B
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus, 1% Secant 283 MPa
41000 psi
ASTM D790
Izod Impact, Notched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point <= 253 °C
<= 487 °F
Peak Melting Point; ExxonMobil method
Users viewing this material also viewed the following: