ExxonMobil PP1014H1 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP1014H1 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableEthylene Oxide SterilizableLow ExtractablesSteam SterilizableUses: LabwareMedical PackagingMedical/Healthcare ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-2/50
Elongation at Yield 7.0 %
7.0 %
ISO 527-2/50
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-2/1
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched (ISO) 1.99 kJ/m²
0.950 ft-lb/in²
ISO 180/A
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Crystallization Temperature 237 °C
459 °F
ISO 3164
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F
ISO 75-2/A
Vicat Softening Point 152 °C
306 °F
ISO 306/A50