Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ HMT 402 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with very high stiffness, high heat ageing resistance and detergent resistance designed for electrical applications such as washing ma..
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ HMU 202 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and low emissions for automotive HVAC and under-the-hood applications.Availability: Africa & Middl..
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ HMU 208 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and release agent for automotive HVAC and under-the-hood applications.Availability: Africa & Middl..
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ HMU 216 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive exterior applications in which good surface finish and good UV resistance ..
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
ISO 179
ExxonMobil Exxtral™ HMU 405 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with high heat ageing resistance, high transparency, low color and low discoloration for contact with hot water, hot air and detergent..
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
ExxonMobil PP1014H1 Polypropylene Homopolymer
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE..
Charpy Impact, Notched 0.294 J/cm²
1.40 ft-lb/in²
ISO 179/1eA
ExxonMobil PP1064L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..
Charpy Impact, Notched 0.294 J/cm²
1.40 ft-lb/in²
ISO 179
ExxonMobil PPT0170F Polypropylene Homopolymer
Product Description: PPT0170F is an unstabilized homo polymer granular resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation prov..
Charpy Impact, Notched 0.294 J/cm²
1.40 ft-lb/in²
ISO 179/1eA
ExxonMobil PP1364E2 Polypropylene Homopolymer
Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc..