ExxonMobil Paxon™ AL55-003 Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Paxon™ AL55-003 Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: AL55-003 is a blow molding grade high density polyethylene offering a good combination of stiffness and stress crack resistance.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoApplications: Drainage PipesFood packagingHousehold and Industrial chemical containersPharmaceutical Packaging Thermoformed Parts Thin Gauge SheetInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D4883
ESCR 100% Igepal® 30 hour
30 hour
ASTM D1693 Condition B
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 560 %
560 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 189 kJ/m²
90.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
260 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F