Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 281-55MED Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 281-55MED Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. Prior to release, each medical grade lot undergoes a Cytotoxicity study using the ISO elution method and a Physico-Chemical - Elastomeric Closures test for heavy metals such as lead. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
.12 in; ASTM D2240
Tensile Strength at Break 4.90 MPa
710 psi
Across Flow; ASTM D412
5.434 MPa
788.1 psi
Air at 212°F, 168 hr; ASTM D573
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
Elongation at Break 410 %
410 %
Across Flow; ASTM D412
446.9 %
446.9 %
Air at 212°F, 168 hr; ASTM D573
Tear Strength 5.96 kN/m
34.0 pli
212°F, Die C; ASTM D624
16.0 kN/m
91.0 pli
73°F, Die C; ASTM D624
Compression Set 20 %
20 %
73°F, 168 hr; ASTM D395
48 %
48 %
212°F, 168 hr; ASTM D395
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets
Users viewing this material also viewed the following: