ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS blends for applications where hard/soft combinations are required. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features: Designed for excellent adhesion onto ABS, PS, PC, PMMA and ASA (cold insert or 2K [two-shot] molding).Recommended for applications requiring superior part surface appearance.Designed for soft touch applications.UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.Adhesion values can vary according to type of ABS, PS, PC, PMMA, ASA or blends thereof, tool design and processing conditions.EU and China RoHS compliant.Applications:Automotive – Grips, HVAC Flapper Door Seals, Interior, Electronics, Floor Care, Kitchen Tools, Power Tools, Writing Instruments and Consumer ApplicationsSeals and GasketsSoft Touch GripsUses:Appliance ComponentsAppliancesAutomotive ApplicationsAutomotive Under the HoodBondingCell PhonesConsumer ApplicationsEyeglass FramesFlexible GripsKitchenwareLiving HingesSealsSporting GoodsStrain ReliefsTie-LayerWhite Goods & Small AppliancesProcessing Method: Coextrusion, Injection Molding and Multi Injection MoldingAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
Air at 212°F, 168 hr; ASTM D573
61
61
Air at 257°F, 168 hr; ASTM D573
53

@Thickness 2.00 mm
53

@Thickness 0.0787 in
15 sec; ISO 868
Tensile Strength at Break 1.600 MPa
232.1 psi
Air at 257°F, 168 hr; ASTM D573
2.954 MPa
428.4 psi
Air at 212°F, 168 hr; ASTM D573
4.10 MPa
595 psi
Across Flow; ASTM D412
Tensile Stress 1.00 MPa

@Strain 100 %
145 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 180 %
180 %
Air at 257°F, 168 hr; ASTM D573
516 %
516 %
Air at 212°F, 168 hr; ASTM D573
600 %
600 %
Across Flow; ASTM D412
Compression Set 55 %
55 %
257°F, 70 hr; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -47.0 °C
-52.6 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.10 mm
HB

@Thickness 0.0433 in
HB

@Thickness 2.90 mm
HB

@Thickness 0.114 in
Processing Properties Metric English Comments
Melt Temperature 98.9 - 110 °C
210 - 230 °F
For two-shot injection molding
110 - 121 °C
230 - 250 °F
For insertion injection molding
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets
Users viewing this material also viewed the following: