Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills AP6106-HS Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP6106-HS Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: child protection systems, appliance components, consumer durables, and automotive interior trim.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 1.19 GPa
173 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
23° C; ASTM D256
Gardner Impact 29.0 J

@Temperature -30.0 °C
21.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648