Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® HB4903 Sheet and Thermoforming HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® HB4903 Sheet and Thermoforming HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density Hexene CopolymerApplications: Fuel tanks, seating, garbage cans, sheet, large industrial containers.Formolene HB4903 is a high performance copolymer that is designed for the most demanding blow molding applications. It is also utilized in many sheeting applications. This resin has exceptional stress crack resistance, excellent surface appearance, good melt strength, and good processability.Produced using licensor formulation for HHM 4903. Licensor does not warrant or imply that this product meets their specifications for HHM 4903.Formolene HB4903 meets all the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520 for food packaging at temperatures not exceeding 212°F (100°C).Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 500 hour
500 hour
Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693
500 hour
500 hour
Condition B (10% Igepal), F<sub>50</sub>; ASTM D1693
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 600 %
>= 600 %
2" (50mm) per min.; ASTM D638 Type IV
Thermal Properties Metric English Comments
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746