Material Notes:
Acrylonitrile Butadiene Styrene copolymer has a good thermal and dimensional stability and scratch resistance. Advantagesgood mechanical strengthresists scratchinghigh surface strengthhigh impact strengthlow Moisture absorptionhigh dimensional stabilitynot weather resistantlimited resistance to alkalines and acidsApplicationsFood industryRefrigeration industry
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Water Absorption 0.40 %
0.40 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
Hardness, Shore D 70
70
DIN 53505
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Modulus of Elasticity 2.26 GPa
328 ksi
ISO 527
Flexural Strength 67.0 MPa
9720 psi
3.5%; ISO 178
Charpy Impact Unnotched 33.3 J/cm²
158 ft-lb/in²
ISO 179
Charpy Impact, Notched 3.70 J/cm²
17.6 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ISO 75
Vicat Softening Point 103 °C
217 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Acid Resistance yes
Aromatic Resistance no
Bondability yes
CKW Resistance no
Color Natural
Hydrocarbonate Resistance limited
Hydroxide Resistance no
Ketone Resistance limited
Physiological indifference according no
Resistance Against Hot Water limited
UV Stabilization no