GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer GEHR Plastics Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ISO 1183
Water Absorption 5.5 %
5.5 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 527
Elongation at Break 12 %
12 %
ISO 527
Modulus of Elasticity 3.20 GPa
464 ksi
ISO 527
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
VDE 0303
Surface Resistivity per Square >= 1.00e+12 ohm
>= 1.00e+12 ohm
VDE 0303
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
VDE 0303
Dielectric Loss Index 0.040

@Frequency 1.00e+6 Hz
0.040

@Frequency 1.00e+6 Hz
DIN 53483
Descriptive Properties Value Comments
Aromatic Resistance limited
Color Black
Hydrocarbonate Resistance limited
Ketone Resistance limited
Resistance Against Hot Water limited