Polymer Property : Thermal Conductivity = 1.20 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.20 W/m-K

@Temperature 100 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 42 Dense Refractory Brick
Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c..
Thermal Conductivity 1.20 W/m-K

@Temperature 650 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast B Sp Dense Refractory Brick
Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples ..
Thermal Conductivity 1.20 W/m-K

@Temperature 1100 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast C Dense Refractory Brick
Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 1300 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 1000 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 1300 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable
Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable
Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable
Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide..
Thermal Conductivity 1.20 W/m-K

@Temperature 100 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast A 1 S Dense Refractory Brick
Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai..
Thermal Conductivity 1.20 - 1.30 W/m-K

@Temperature 100 °C
8.33 - 9.02 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable
Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi..
Thermal Conductivity 1.20 W/m-K

@Temperature 600 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 1110 °F
EN 993-15 1998
Skamol Group SKAMOBAR 69 Low-Alumina Fireclay Brick
Low-alumina fireclay brick has the following characteristics: Max. service temperature 1100°C (2012°F)For barrier lining of aluminum reduction cellsExcellent cryolite resistanceLow thermal con..