Material Notes:
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 D has a very good resistance against erosion and corrosion. It is specially applied in electric arc furnace roofs.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 1.31 - 1.51 W/m-K

@Temperature 100 °C
9.09 - 10.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.38 - 1.58 W/m-K

@Temperature 600 °C
9.58 - 11.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.48 - 1.68 W/m-K

@Temperature 1600 °C
10.3 - 11.7 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 1760 °C
3200 °F
Shrinkage -0.700 - 0.300 %

@Temperature 1600 °C
-0.700 - 0.300 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
Fe2O3 1.0 %
1.0 %
SiO2 8.0 %
8.0 %
Descriptive Properties Value Comments
Bonding Type ceramic
Material Consumption per 1 m3 2650 kg
Mixing Water 8-10 liters per 100 kg dry material
Segercone 41