Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1760 °C
3200 °F
Pyrotek Pyrocast ZI Refractory Shapes
Aggregate Base: BauxiteApplicationsCrucible bottoms Information provided by Pyrotek.
Maximum Service Temperature, Air 1760 °C
3200 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 94 M Dense Refractory Brick
Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â..
Maximum Service Temperature, Air 1760 °C
3200 °F
Gouda Vuurvast AK 94 M Dense Refractory Brick
Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â..
Maximum Service Temperature, Air 1760 °C
3200 °F
Gouda Vuurvast CURAS 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund..
Maximum Service Temperature, Air 1760 °C
3200 °F
Gouda Vuurvast CURAS 90 Moldable Refractory Material
Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an..
Maximum Service Temperature, Air 1760 °C
3200 °F
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..
Maximum Service Temperature, Air 1760 °C
3200 °F
Normal oxidizing atmosphere
BNZ Materials BNZ-32 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Ceramabind™ 644-S High Temperature Inorganic Binder
A colloidal silica aqueous solution which produces high adhesive strength. Ideal for blending with all types of granular and fibrous ceramics. Excellent resistance to temperature, moisture and mecha..
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina
Coarse grain castable for producing large hi-temp tooling.
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C)
Maximum Service Temperature, Air 1760 °C
3200 °F
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating
This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200..