Polymer Property : Thermal Conductivity = 1.38 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.38 W/m-K

@Temperature 1100 °C
9.58 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast A Vuurvast Dense Refractory Brick
Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that ..
Thermal Conductivity 1.38 W/m-K

@Temperature 650 °C
9.58 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 46 S Dense Refractory Brick
Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05%..
Thermal Conductivity 1.38 W/m-K

@Temperature 650 °C
9.58 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 50 Dense Refractory Brick
Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato..
Thermal Conductivity 1.38 W/m-K

@Temperature 1100 °C
9.58 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast B 1 Sp Dense Refractory Brick
Description: High mechanical strength and very low porosity are typical for this type of brick. Application: transition zone in cement kilns, incinerators, steel ladles.Remarks: This data represents..
Thermal Conductivity 1.38 - 1.58 W/m-K

@Temperature 600 °C
9.58 - 11.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund..
Thermal Conductivity 1.38 - 1.48 W/m-K

@Temperature 1300 °C
9.58 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 170 Dense Refractory Castable
Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v..
Thermal Conductivity 1.38 - 1.48 W/m-K

@Temperature 1300 °C
9.58 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 170 GM Dense Refractory Castable
Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:..