Gouda Vuurvast CURON 160 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 160 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal shock resistance. It is largely used in the steel industry.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.45 - 2.55 g/cc
0.0885 - 0.0921 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1400 °C
5080 - 6530 psi

@Temperature 2550 °F
Cold Crushing Strength
50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.750 - 0.850 W/m-K

@Temperature 100 °C
5.20 - 5.90 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.800 - 0.900 W/m-K

@Temperature 600 °C
5.55 - 6.25 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.930 - 1.03 W/m-K

@Temperature 1400 °C
6.45 - 7.15 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.550 - 0.550 %

@Temperature 1400 °C
-0.550 - 0.550 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 64 %
64 %
CaO 3.5 %
3.5 %
Fe2O3 1.0 %
1.0 %
SiO2 30 %
30 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2450 kg
Mixing Water 8-10 liters
per 100 kgs dry material
Copyright © lookpolymers.com All Rights Reserved