Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1300 °C |
5080 - 6530 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1300 °C |
5080 - 6530 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1400 °C |
5080 - 6530 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1000 °C |
5080 - 6530 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 L Dense Refractory Castable Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1000 °C |
5080 - 6530 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by .. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1300 °C |
5080 - 6530 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 C Dense Refractory Castable Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information .. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1300 °C |
5080 - 6530 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 Dense Refractory Castable Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products... |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1400 °C |
5080 - 6530 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 Dense Refractory Castable Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 100 °C |
5080 - 6530 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 165 GM Dense Refractory Castable Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo.. |
|||
Compressive Strength | 35.0 - 45.0 MPa @Temperature 1600 °C |
5080 - 6530 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |