Polymer Property : Compressive Strength = 35.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 35.0 MPa

@Strain 1 %
5080 psi

@Strain 1 %
ISO 604
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data)
Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good ..
Compressive Strength 35.0 MPa

@Strain 1 %
5080 psi

@Strain 1 %
ISO 604
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data)
Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp..
Compressive Strength 35.0 MPa

@Temperature 200 °C
5080 psi

@Temperature 392 °F
ISO 604
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 140 Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 140 Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable
This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1400 °C
5080 - 6530 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1000 °C
5080 - 6530 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 FS Dense Refractory Castable
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable
Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 L Dense Refractory Castable
Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable
Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1000 °C
5080 - 6530 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable
Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by ..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 C Dense Refractory Castable
Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information ..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1300 °C
5080 - 6530 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 Dense Refractory Castable
Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products...
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1400 °C
5080 - 6530 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 Dense Refractory Castable
Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable
Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 165 GM Dense Refractory Castable
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo..
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1600 °C
5080 - 6530 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable
Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply ..
Compressive Strength 35.0 MPa

@Temperature 200 °C
5080 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..